1. Why it bends: It all comes down to one thing
The essence of bending is "uneven distribution of internal stress + asymmetry in external force/thermal effect". During the processes of pipe forming, welding, and heat treatment, if there is a temperature gradient, deformation difference, or microstructure difference in the circumferential or longitudinal direction at any stage, it will leave asymmetric residual stress inside the pipe; after the stress is released, the pipe will bend towards the side with less stress.
You can think of it this way: The "sides" of the pipe wall contract/deform differently. It's like a wet board where one side dries faster than the other. Once it dries, it naturally curls.
II. Which production steps have gone wrong (identify each step one by one)?
| Step | Typical causes | Signs |
| Raw materials | Residual stress from plate rolling has not been released; composition segregation (uneven C, Mn); | lateral wall thickness difference After forming into a pipe, stress is released and the entire pipe bends spontaneously |
| Forming (priority) | Forming rolls wear, uneven pressing force, deviation of the center line of the mold; insufficient unwinding tension, skew of the feeding guide plate causing the steel strip to enter the forming zone at an angle; insufficient pre-bending, unreasonable JCO spacing / die opening | Uneven extension on both sides of the pipe billet, cumulative bending deviation from the first pass, severe cases may result in spiral twisting deformation |
| Welding (most prominent) | Single-sided welding with concentrated heat input, cooling contraction of the weld seam is much greater than that of the base material, the pipe bends towards the weld seam (i.e. "welding bend"); uneven heat input on both sides of the double-sided weld; asymmetrical excess height of the weld seam inside and outside forming a "rib effect"; mismatch of pipe end welding deformation causing the end to curl up |
Directional bending towards the weld seam |
| Heat treatment / cooling | Local water cooling (such as manual thermal inspection with local water spraying), large temperature difference between up/down/left/right | Thermal difference → thermal stress → overall bending |
| Reamming / water pressure | Improper reaming parameters, uneven axial strain rate; residual stress redistribution after water pressure test | Exposure of potential bending or generation of new deformation |
| Straightening itself | Misalignment or severe wear of the straightening rollers, inconsistent pressure between the three rollers, and too large a distance between the rollers | More straightening → more bending / end bending / local non-roundness |
| Diameter control machine | Unreliable equipment calibration, improper assembly and adjustment | Excessive bending occurs immediately after line output |
| Lifting / stacking | Insufficient support points for long pipes (few lifting points), excessive stacking layers |
Weight causes plastic bending due to gravity (external cause) |
To supplement an industry consensus: Due to the fact that almost all rollers on the production line cannot be perfectly aligned in a straight line, the smaller deviations in the arrangement of the rollers for longer pipes are more likely to be amplified into obvious bends - this is the inherent amplification factor for the bending of large-diameter long pipes, and also the reason for adding roll spacing and the number of rolls in the subsequent straightening plan.
III. How to Avoid (Prevention takes priority, full-chain control)
- Source: Control the residual stress of the plate strip and the uniformity of wall thickness, and inspect the lateral wall thickness difference before feeding;
- Forming: Ensure the alignment of the mold and the accuracy of the roller system, ensure sufficient pre-bending, reasonable JCO parameters, stable unwinding tension, and no deviation in feeding;
- Welding: Control the symmetry of heat input on the inner and outer sides, ensure sufficient annealing treatment of the weld seam (insufficient annealing will result in residual heat stress on the weld seam side, which bends in the same direction as the weld seam after cooling); Ensure uniform weld seam height;
- Cooling/Heat Treatment: Avoid local rapid cooling, keep the temperature difference during equal heating within 15℃, and ensure uniform wind speed on the cooling bed;
- Straightening Machine Maintenance: Replace the straightening rollers in time, keep the pressure and roller angle of the three rollers consistent;
- Layout: Increase the number and spacing of forming/welding rollers to offset the cumulative deviation of the roller line;
- Logistics: Use multiple points of support for hoisting (long pipes ≥ 2 support points), control the stacking layer, and store neatly.